Lithium plating detection and degradation analysis on EEMB LIR-2032 graphite||LiCoO2 coin cells
0.029Charge Throughput Decrease RateGaussian Process (GP) framework
Evaluation Results
| Method | Links | ||||
|---|---|---|---|---|---|
| Gaussian Process (GP) frameworkOperating condition=0.2 C@0 ◦C2025.09 | 0.029 | — | — | 0.094 | |
| Gaussian Process (GP) frameworkOperating condition=1.0 C@40◦C2025.09 | 0.093 | — | — | 0.016 | |
| Gaussian Process (GP) frameworkOperating condition=1.0 C@25◦C2025.09 | 0.227 | — | — | 0.031 | |
| Gaussian Process (GP) frameworkOperating condition=1.0 C@10◦C2025.09 | 1.464 | — | — | 0.877 | |
| Gaussian Process (GP) frameworkOperating condition=0.4 C@10◦C2025.09 | 1.671 | — | — | 1.237 | |
| Gaussian Process (GP) frameworkOperating condition=0.4 C@0 ◦C2025.09 | 1.711 | — | — | 0.845 | |
| Gaussian Process (GP) frameworkOperating condition=0.6 C@0 ◦C2025.09 | 3.617 | — | — | 1.175 |