# Optical and Electrical Characterization of Boron-Doped Diamond

Source: [Optical and Electrical Characterization of Boron-Doped Diamond](<https://www.sota2.com/research/paper/68fa2bf61e209131ce84bb56>)

Collection index: [llms.txt](<https://www.sota2.com/research/llms.txt>)

Data updated: 2025-10-24T15:02:21.105Z

Authors: Sunil K. Karna, Yogesh. K. Vohra, Samuel T. Weir

Published: 2012-10-29T21:45:17.000Z

## Abstract

The boron-doped single crystal diamond films were grown homoepitaxially on synthetic (100) oriented Type Ib diamond substrates using a Microwave Plasma Chemical Vapor Deposition (MPCVD) technique. Raman spectrum showed a few additional bands at the lower wavenumber regions along with the zone center optical phonon mode for diamond. The change in the peak profile of the zone center optical phonon mode and its downshift were observed with the increasing boron content in the film. A modification in surface morphology of the film with increasing boron content had been observed by atomic force microscopy. Four point probe electrical measurement indicated that different conduction mechanisms are operating in various temperature regions for these semiconducting films.

## Recorded benchmark results

A research result applies to its stated dataset, split, metric and evaluation configuration. Compare like-for-like settings, preserve the metric's unit and direction, and distinguish paper-reported results from independent reproduction. The best result recorded here is not a claim of exhaustive, current global coverage.

## Original sources and implementation

[Original paper](<https://arxiv.org/abs/1210.7846>)

[PDF](<https://arxiv.org/pdf/1210.7846.pdf>)